Fig. 2: Single fibre diffraction pattern recorded at a reeling speed of 0.36 cm s­1 during forced silking with a CCD detector. The strongest equatorial reflections have been indexed.

back to: In situ Studies of Forced Silking of Nephila Senigalensis Spiders