Fig. 92: Equiaxed dendritic growth of Pb crystals in an Sn-52wt%Pb alloy. Thermal gradient, (T/z)global ~ 29.5 K/mm, sample translation ||z = -9.6 µm/s, 1.0 s exposure. Positive z points vertically upwards. Sample-detector distance 75 cm. (a) t0, (b) 3 frames later, t0 + 4.5 s.