Fig. 28: Magnetic (0, 0, 2) - satellite and (0, 0, 2) Bragg reflection measured in a 370 Å thick holmium film grown epitaxially on a W(110) single crystal. Shown is the intensity in the rotated - polarisation channel at 40 K.